1.Heart hardness: standard value HRC28-38. The test is carried out on a section 1-2 times the nominal diameter from the tail. If the nominal length is too short, it can be embedded first, and then the hardness is measured.
2.Surface hardness: standard MIN HV450.
3.carburized layer: standard 4#-6#: 0.05-0.18mm, 8#-12#: 0.10-0.23 mm, 14#: 0.13-0.28 mm. The main purpose of carburizing is to increase the surface hardness and ensure the strength of the teeth. If the decarburization is too deep and the carburizing is insufficient, the strength of the teeth will not meet the requirements, that is, the teeth will be damaged during the screwing test.
4.torque: standard specification 4#5#6#7#8#10#12#14#A tooth 14212835455696145AB tooth 142128354565102165.
1. Heart hardness: standard value HRC28-38. The test is carried out on a section 1-2 times the nominal diameter from the tail. If the nominal length is too short, it can be embedded first, and then the hardness is measured.
2. Surface hardness: standard MINHV450.
3. Carburized layer: standard 4#-6#: 0.05-0.18mm, 8#-12#: 0.10-0.23mm, 14#: 0.13-0.28mm. The main purpose of carburization is to increase the surface hardness and ensure the strength of the teeth. If the decarburization is too deep and the carburization is insufficient, the strength of the teeth will not meet the requirements, that is, the teeth will be damaged during the screwing test.
4. Torque: standard specification 4#5#6#7#8#10#12#14#A tooth 14212835455696145AB tooth 142128354565102165.